Armox is a high performing protection plate for environments where personal safety is crucial. It’s tough and strong and goes through extensive ballistic testing to meet stringent international criteria.
Armox 600T is used as an add-on protection plate or where weight is critical. It is particularly suitable for VIP vehicles and security doors.
Armox 500T is the world’s toughest protection plate in its hardness range. It can be used in many applications including vehicles and static structures such as buildings. It is very easy to work with and requires no special processing skills.
Armox 440T represents a new generation of protection plate, particularly against blast. It provides vehicle designers with new possibilities of increasing protection with lighter weight designs.
Armox 370T Class 1 is traditional “rolled homogeneous armour” RHA, with excellent ballistic properties in combination with good workability, and is used in many vehicle applications.
Armox 370T Class 2 combines good ballistic properties with excellent toughness. It is very suitable for blast protection and can be easily welded and offers excellent bendability.